Convert Rockwell HRC & HRB, Brinell HBW, Vickers HV, and tensile strength (MPa / ksi) per ASTM E140 with searchable table, steel grades, and QC notes.

Rockwell C (HRC)—150 kgf Diamond Cone
Brinell (HBW 10/3000)—10 mm Carbide Ball
Vickers (HV)—136° Diamond Pyramid
Approx. Tensile (UTS)——
Typical Grade: EN24 / AISI 4340 Q&T Shaft — Carbide roughing OK
HRCHRBHBW (10/3000)Vickers HVTensile (MPa / ksi)Typical Steel & Shop Note
Embed this free tool on your website or blog

Free to embed on engineering blogs, university guides, and plant wikis (zero login required).

HRC 150 kgf Cone Needs >1.0 mm case HBW 10 mm Ball Best for forgings/castings Vickers HV (1–10 kgf) Nitrided & thin cases

Matching indenter load to case depth prevents anvil/core punch-through on hardened shafts.

QC Floor Rule: Check HBW Before Blaming CNC Inserts

When a lathe operator burns through carbide inserts on incoming 4140 / EN19 bar stock, grab a portable Brinell or Leeb tester before tweaking cutting speeds. Normal annealed 4140 sits around 197–229 HBW. Mill-quenched stock that missed tempering often arrives at 340–380 HBW (37–41 HRC) and chips standard P25 carbide on the first pass.

Dive deeper into heat treatment in our Metallurgical Engineering Guide and turning speeds in our Lathe Machines Guide.

Where ASTM E140 Breaks Down

  • Austenitic Stainless (304/316): Rapid work-hardening makes HRC vs HBW tables inaccurate by 10–15%.
  • Bearing Races & Shaft Fits: Typical 52100 races run 60–64 HRC; verify shaft/housing hardness when specifying SKF / FAG Bearing fits.
  • Fastener Verification: ISO Class 10.9 bolts sit at 32–39 HRC (check Bolt Torque Chart).

Frequently Asked Questions

When is Rockwell C (HRC) vs Brinell (HBW) or Vickers (HV) the right test?

Use HRC (150 kgf diamond cone) on hardened tool steels, shafts, and gears above 20 HRC. Use Brinell HBW (10 mm ball, 3000 kgf) on raw castings, forgings, and annealed bar stock. Use Vickers HV (low load 1-10 kgf) on thin nitrided or induction-hardened cases.

Why does ASTM E140 warn against converting hardness on 304/316 stainless or cast iron?

ASTM E140 Table 1 applies strictly to non-austenitic carbon and alloy steels. Austenitic 304/316 stainless work-hardens under the indenter, while flake graphite in grey cast iron skews ball vs diamond readings by 15-25%.

Can I convert Brinell HBW directly to approximate tensile strength?

For carbon and low-alloy steels under ~350 HBW, Ultimate Tensile Strength (MPa) is roughly 3.45 x HBW (or ~0.50 x HBW in ksi). Always pull a tensile bar for ASME pressure vessel or structural certification.

Why did my 58 HRC induction-hardened shaft read 38 HRC on a Rockwell tester?

A 150 kgf HRC diamond cone penetrates ~0.08-0.12 mm and needs at least 10x that depth in case thickness (~1.0 mm minimum) so the soft core does not collapse underneath. Thin cases require HR15N superficial Rockwell or micro-Vickers HV.

Jignesh S Panchal
Technical Editorial Author Verified Editor

Jignesh S Panchal

Founder — Jaadu Digital & Musafir Infotech · 9+ Years in Industrial B2B

Jignesh S Panchal is the founder of Jaadu Digital and Musafir Infotech, and the publisher behind EngiTech. With over 9 years of hands-on experience in industrial marketing and B2B growth, he works closely with machinery OEMs, process equipment manufacturers, and industrial service providers across thermal processing, fluid handling, automation, packaging, and plant reliability. Combining deep practical knowledge of industrial manufacturing with how technical buyers actually evaluate equipment, he built EngiTech to give plant engineers and procurement teams reliable sizing tools, fault diagnostics, and verified B2B supplier discovery.

Your saved guides

Saved only in this browser. No account required.

Advertisement